Abstract:The infrared stealth coatings was prepared by using modified fluorocarbon resin as bond,graphite as stuffing.As a result,after adding 25% (mass percent)graphite into bond,with the 2μm grain size of graphite,the emissivity of the infrared stealth coatings was 0.63.The adhesive attraction of coatings was first-order,the resistance to impact was higher than 50 kg·cm,the acid resistivity,alkali resistivity and salt water resistivity was well.